Catalytic activity of Au-Cu/CeO2-ZrO2 catalysts in steam reforming of methanol

Authors: Chinchanop Pojanavaraphan, Apanee Luengnaruemitchai, Erdogan Gulari

Abstract:
Bimetallic Au-Cu/Ce0.75Zr0.25O2 catalysts prepared by deposition–precipitation were tested for steam reforming of methanol(SRM)in the range of 200–500C. Many effective parameters—Au/Cu atomic ratio, gas pretreatment, total metal loading, and calcination temperature—were investigated and correlated with catalyst properties. At the Au/Cu ratio of 1/3, the homogeneous Au–Cu alloy was found to be active for SRM, while an inhomogeneous or partially developed alloy formation was found after applying H2 and O2 pretreatments. There were no significant differences in catalytic activity with different total loadings and calcination temperatures; however, the 7 wt% Au-Cu catalyst calcined at 300 ◦C exhibited complete methanol conversion, 82% H2 selectivity, and 1% CO selectivity at a low temperature of 300C. In regards to stability, the bimetallic catalyst displayed a long life, even though coke and metallic copper were formed.

Keywords:
Steam reforming of methanol
Hydrogen
Alloy
Bimetallic
Au catalyst

Published in: Applied catalysis A: General  (Volume 456, Pages 1-248, 10 April 2013)

Publisher: Elsevier

ISSN Information: 0926-860X

Catalytic activity of Au-Cu/CeO2-ZrO2 catalysts in steam reforming of methanol

Bình luận của bạn
*
*
*
*
 Captcha

Logo Bottom

Địa chỉ: 268 Lý Thường Kiệt, P.14, Q.10, TP.HCM           Tel: 38647256 ext. 5419, 5420           Email: thuvien@hcmut.edu.vn

© Copyright 2018 Thư viện Đại học Bách khoa Tp.Hồ Chí Minh 

Thiết kế website Webso.vn